عنوان المقالة:Effect of Electrical Discharge Energy on White Layer Thickness of WEDM Process In Reference Module in Materials Science and Materials Engineering
ابراهيم ماهر | Ibrahem Maher | 13467
نوع النشر
مجلة علمية
المؤلفون بالعربي
Ibrahem Maher, Ahmed A. D. Sarhan, Houriyeh Marashi
الملخص العربي
One of the major requirements of wire electrical discharge machining (WEDM) is to develop suitable technology for producing smooth surfaces. The main characteristic of WEDM is the development of the white layer. To ensure good surface quality, the white layer thickness (WLT) must be as thin as possible, homogeneous, and crack-free. Spark energy and wire electrode type are the most important parameters to experimentally investigate WLT. Experimental results show that the WLT increases linearly by 3 and 2 µm for every 20-µJ increase in the spark energy while using brass and coated wire, respectively.
تاريخ النشر
01/12/2016
الناشر
Elsevier
رابط خارجي
http://www.sciencedirect.com/science/article/pii/B9780128035818091542
الكلمات المفتاحية
AISI 1050 carbon steel, ANFIS modeling, Brass wire, Coated wire, Electrical discharge energy, Heat-a